IMDEA Materials has installed the first dedicated high temperature nanoindentation instrument in Spain
February 8, 2013
This instrument allows nanoindentation to be carried out at temperatures up to 750°C, and also in inert environments. The instrument uses both tip and sample heating, ensuring stability for long duration testing, including creep tests. More info ….(+)